Albond 5 Si (E4043)
Albond 5 Si (E 4043)
- Special coated electrode
- Keep short arc to avoid burn through and excessive spattering
- Electrode dia. should roughly be equivalent to plate thickness
- Provide high melting rate
- Slag residues should be thoroughly removed to obtain non corrosive weld
- Section thickness above 8 mm should be preheated to min. 200ºC
- Fabrication and repair of wrought and cast Al alloys with Si upto 7%
- Welding of similar grade Al alloys in the form of pipe, plate, forging and casting